Ramli, Rusydi Aiman (2026) Exploring the wood cascading potential of urea formaldehyde- and citric acid-bonded composites. Masters thesis, Universiti Teknologi MARA (UiTM).
Abstract

The presence of synthetic adhesives, particularly urea–formaldehyde (UF), represents a major barrier to the cascading utilization of wood composites. In contrast, citric acid (CA) has emerged as a promising bio-based adhesive with potentially greater compatibility with recycling processes. Nevertheless, comprehensive studies on the recyclability of CA-bonded wood composites remain limited, and their suitability for multi-stage cascading has yet to be fully established. Therefore, the general objective of this study was to evaluate the wood-cascading potential of CA-bonded composites in comparison with conventional UF-bonded composites through successive conversion into particleboard and fibreboard. The feasibility of multiple cascading stages was demonstrated for both adhesive systems based on compliance to JIS A 5908 and JIS A 5905 for particleboard and fibreboard, respectively. Although the initial approach aimed to retain the original adhesive systems throughout recycling, the rebonding performance of CA was found to be inferior irrespective of recycled particle type, leading to the adoption of UF resin as the primary binder for recycled boards. Untreated recycled particles exhibited poor bonding performance due to residual adhesive fragments, necessitating surface modification. Among the treatment strategies investigated, hydrothermal treatment in water at 120 °C proved most effective in removing residual UF and CA contaminants and enhancing composite performance. Excessive temperature (150 °C) resulted in severe particle degradation, while sodium hydroxide treatment caused structural damage and reduced dimensional stability. A board density of at least 600 kg/m³ was required to meet the minimum physical and mechanical requirements specified in JIS A 5908. While UF-based systems consistently exhibited superior mechanical properties, CA-based systems demonstrated improved thickness swelling resistance. Chemical and morphological analyses confirmed effective residue removal following hydrothermal treatment, as evidenced by reduced nitrogen content for UF and altered carbon–oxygen ratios for CA in FESEM–EDX observations. Improved rebonding led to substantial increases in modulus of rupture, modulus of elasticity, and internal bond strength; however, increased thickness swelling was attributed to cell-wall relaxation and springback phenomena. Material efficiency assessment indicated higher cascading potential for UF-bonded composites, enabling up to 50% recycled content while maintaining acceptable performance, compared to 30% for CA-based systems. The cascading factors of 1.518 (UF) and 1.471 (CA) confirmed successful multi-stage circular utilization. Although CA systems exhibited slightly lower cascading efficiency, their inherent environmental advantages support their continued development as sustainable adhesive alternatives.

Item Details
Edit Item
Edit Item
Downloads & Files
[thumbnail of 150687_fulltext.pdf]
Text
150687_fulltext.pdf
Available under License Dasar Harta Intelek UiTM (Para 6).
Download (1MB)
[thumbnail of declarationform.pdf]
Text
declarationform.pdf
Restricted to Repository staff only
Download (596kB)
Location & Physical Holdings
Digital Copy
Physical Location
Item Status
Indexing & Metrics