Deadhesion mechanism of commercial unpigmented epoxy and alkyd coating under cathodic polarisation / M.K. Harun and M.Z.A. Yahya

Harun, M.K. and Yahya, M.Z.A. (2005) Deadhesion mechanism of commercial unpigmented epoxy and alkyd coating under cathodic polarisation / M.K. Harun and M.Z.A. Yahya. Science Letters, 2 (1). pp. 1-11. ISSN 1675-7785

Download

[thumbnail of AJ_M.K. HARUN SL 05.pdf] Text
AJ_M.K. HARUN SL 05.pdf

Download (481kB)

Abstract

The wet adhesion behavior of epoxy-polyamide, and alkyd organic coating on silane modified mild steel surface has been studied in an earlier work. Results indicated that 3-
Glycidoxypropyltrimethoxy silane (3-GPS) enhanced the wet adhesion of epoxy-polyamide coating and 3-Aminopropyltrirthoxy silane (3-APS) enhanced the wet adhesion of alkyd coating with cohesive failure mode towards the end of the experiment. Cathodic disbonding
experiments on these systems indicated that the enhanced adhesion for alkyd, has no effect on their cathodic disbonding behaviour while the use of 3-GPS to enhanced the adhesion of epoxy-polyamide greatly reduced its rate of cathodic disbanding.

Metadata

Item Type: Article
Creators:
Creators
Email
Harun, M.K.
mohamadkamal@salam.uitm.edu.my
Yahya, M.Z.A.
UNSPECIFIED
Subjects: Q Science > QD Chemistry > Physical and theoretical chemistry
Divisions: Universiti Teknologi MARA, Shah Alam > Faculty of Applied Sciences
Journal or Publication Title: Science Letters
UiTM Journal Collections: UiTM Journal > Science Letters (ScL)
ISSN: 1675-7785
Volume: 2
Number: 1
Page Range: pp. 1-11
Item ID: 11792
Uncontrolled Keywords: Cathodic disbonding, epoxy-polyamide, alkyd, 3-Aminopropyltrirthoxy silane, 3-Glycidoxypropyltrimethoxy silane, wet adhesion
URI: https://ir.uitm.edu.my/id/eprint/11792